Why high-alloy material shearing machine blades need to be tempered multiple times
May 09, 2026
Why high-alloy material shearing machine blades need to be tempered multiple times: High-alloy blades that are quenched at high temperatures need to be tempered multiple times. 

For example, medium-thick plate shears made of H13 (4Cr5MoSiV1) steel require more than two tempers. This is because these high-temperature quenched high-alloy steel blades contain more retained austenite after quenching. The purpose of multiple tempering is to allow the retained austenite to transform into martensite during tempering cooling, and the martensite formed from retained austenite then transforms into tempered martensite. 

If a single long tempering is used, it is difficult to achieve the above structural transformations, resulting in insufficient tempering. This will lead to inconspicuous secondary hardening, poor dimensional stability of the workpiece, higher brittleness, and lower service life. 

Licheng Knife is committed to popularizing industry knowledge for the wide audience of frontline sales professionals!
Boletín de noticias

Por favor, lea, estancia publicado, suscribirse, y le damos la bienvenida para que nos diga lo que piensa.

Deje un mensaje
bienvenido a Licheng
Si usted está interesado en nuestros productos y desea conocer más detalles,por favor deje un mensaje,le responderemos tan pronto como podamos.

Página de inicio

Productos

acerca de

contacto